The fatigue fracture mechamism of a typical machinable glass ceramic under static, dynamic and cyclic loading was investigated. 系统研究了在静载荷、动载荷及循环载荷的作用下,一种典型可切削玻璃陶瓷的疲劳断裂机理。
The effect of K 2O and ZrO 2 on crystallization and microstructure in the machinable glass ceramic system of CaO MgO Al 2O 3 SiO 2 F were investigated and also, the mechanism of crystallization of the parent glass was discussed in detail. 在CaOMgOAl2O3SiO2F系可切削微晶玻璃体系中,本研究分析了K2O和ZrO2对玻璃析晶和显微结构的影响,探讨了晶化机理。
The melting and subsequent crystallizing process are key steps in the preparation of machinable glass ceramic. The chemical compositions has a significant effect on them. 玻化和结晶过程是可加工陶瓷制备过程中重要的环节.本文研究了化学成分对玻化和结晶阶段的影响,在玻化阶段希望得到均匀的玻璃熔体,并且冷却过程中不出现晶化;
Microstructure and Properties of a Machinable Glass Ceramic(MGC) with Low Melting Temperature 低熔点可切削微晶玻璃的组织与性能
Growth Behavior of Indentation Crack in a Machinable Glass ceramic 玻璃陶瓷压痕裂纹扩展特性